開発したFSCC06 Serective Spray Coaterの検証結果でさらに大きな効果が期待される。
溶剤系の防湿剤を希釈しないで、30ミクロ前後の成膜をした場合、乾燥時間は従来の半分以下、乾燥温度も下げて乾燥可能になる。
結果として、希釈溶剤30%以上削減、乾燥時間短縮、乾燥温度低減、ピン足エッジ部の塗膜厚大幅アップが得られる。
The bigger effect is expected by an inspection result of developed FSCC06 Serective Spray Coater.
The case and the drying period when a desiccant of an agent course wasn't diluted and film-forming of 30 micro-context was done, conventional, the dryness temperature is also lowered in the following half of, and, it's possible to dry, it'll be.
Drying time reduction, drying temperature reduction and a coating film substantial rise of pin leg edge portion reduce more than 30 % of dilution agent as a result, and are obtained.
<a href="http://business.blogmura.com/seizougyou/ranking.html" target="_blank"><img src="http://business.blogmura.com/seizougyou/img/originalimg/0000526113.jpg" width="162" height="242" border="0" alt="にほんブログ村 企業ブログ 製造業へ" /></a><br /><a href="http://business.blogmura.com/seizougyou/ranking.html" target="_blank">にほんブログ村</a>